Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review
Original language | English |
---|---|
Title of host publication | VII International Young Researchers'' Conference - Physics, Technology, Innovations, PTI 2020 |
Editors | Vladimir A. Volkovich, Ilya V. Kashin, Andrey A. Smirnov, Evgeniy D. Narkhov |
Publisher | American Institute of Physics Inc. |
Number of pages | 5 |
ISBN (Electronic) | 9780735440531 |
DOIs | |
Publication status | Published - 9 Dec 2020 |
Event | 7th International Young Researchers'' Conference on Physics, Technology, Innovations, PTI 2020 - Ekaterinburg, Russian Federation Duration: 18 May 2020 → 22 May 2020 |
Name | AIP Conference Proceedings |
---|---|
Volume | 2313 |
ISSN (Print) | 0094-243X |
ISSN (Electronic) | 1551-7616 |
Conference | 7th International Young Researchers'' Conference on Physics, Technology, Innovations, PTI 2020 |
---|---|
Country/Territory | Russian Federation |
City | Ekaterinburg |
Period | 18/05/2020 → 22/05/2020 |
ID: 20400711